Stay Brite solders bond with all of the ferrous and nonferrous alloys. Joints soldered with Stay Brite solders exhibit considerably higher than necessary elongation for sound, dissimilar metal joints and vibration applications. Both Stay Brite and Stay Brite 8 produce an overall component with greater strength than a brazed component whose base metals are weakened by annealment from high brazing heat.
Harris® Stay Brite® Solder Wire, 1 lb Net Content, Spool Container, 1/8 in Wire Diameter, 450 deg F Melting Point, Silver/Tin
Container Type | : | Spool |
Material | : | Silver/Tin |
Melting Point | : | 450 deg F |
Net Content | : | 1 lb |
Wire Diameter | : | 1/8 in |