All-purpose brazing and soldering of aluminum fittings, castings, tubing, and coils. 600 deg flow temp allows the technician to successfully fix and fabricate all aluminum-grade.
SOLDERWELD® Repair and Joining Rod, 18 in L, Composition: 5% Silicon, 0.3% Iron, 0.001% Copper, 0.003% Magnesium, 0.04% Manganese, 0.003% Zinc, 0.004% Titanium, 94.649% Aluminum, For Joining Material: Aluminum
Composition | : | 5% Silicon, 0.3% Iron, 0.001% Copper, 0.003% Magnesium, 0.04% Manganese, 0.003% Zinc, 0.004% Titanium, 94.649% Aluminum |
For Joining Material | : | Aluminum |
Length | : | 18 in |
SOLDERWELD® SW-AS09305K